MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Wacker ELASTOSIL® R 427/60 High Strength Silicone Base
Categories: Polymer; Thermoset; Silicone; Silicone Rubber; Liquid Silicone Rubber (LSR)

Material Notes: ELASTOSIL® R 427/60 is a High Strength Base noted for its exceptional transparency excellent tear strength and excellent mechanical properties. ELASTOSIL® R 427/60 can be used for extruded profiles. ELASTOSIL® R 427/60 vulcanizing characteristics make it possible to achieve short cycle times in the production of molded articles by compression transfer and injection molding. Post-cured vulcanizates can be used for applications in the health care and food handling industries.

Special features: ELASTOSIL® R 427/60 contains those ingredients which are suitable for food contact*. *Under Title 21 "Food and Drugs," Part 177.2600, "Rubber articles intended for repeated use." Because this regulation contains limitations, compliance to the regulation is the responsibility of the user.

Key Characteristics:

  • Excellent extrusion qualities
  • Excellent molding qualities
  • Excellent tensile strength & tear resistance
  • Excellent clarity

Information provided by Wacker.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.10 - 1.80 g/cc1.10 - 1.80 g/cc
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6060ASTM D746
Tensile Strength 11.0 MPa1600 psiASTM D2240
Elongation at Break 600 %600 %ASTM D412
Tear Strength 43.8 kN/m250 pliDie B; ASTM D412
Compression Set 25 %
@Temperature 177 °C,
Time 79200 sec
25 %
@Temperature 351 °F,
Time 22.0 hour
Method B; WSTM 1114
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %Transparent, but not quantified
 
Processing PropertiesMetricEnglishComments
Cure Time 10.0 min
@Temperature 171 °C
0.167 hour
@Temperature 340 °F
press cured, post cured 4 h/200 °C
 
Descriptive Properties
AppearanceTransparentWSTM 1297

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Wacker Elastosil® LR 3141/50 A/B Liquid Silicone Rubber
Wacker ELASTOSIL® R 407/60 Silicone Rubber Base
Rogers Arlon CP-375CR Silicone Rubber
Rogers Arlon 920-10R##-P-1 Cured Self-Fusing Silicone Rubber Tape
Overview of materials for Silicone Rubber

PWACK9912 / 197511

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.