MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Gilding Copper, UNS C21000, Spring Temper
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Good to excellent corrosion resistance. Excellent cold workability, good hot workability for blanking, coining, drawing, piercing and punching, shearing, spinning, squeezing and swaging, stamping.

Applications: coins, medals, tokens, bullet jackets, firing pin supports, fuse caps, primers, emblems, plaques, base for gold plate.

Available as flat products and wire.

Key Words: CZ125, ISO CuZn5, CEN CW500L, Cap copper, 95/5 brass
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.86 g/cc0.320 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 7373
Hardness, Rockwell 30T 6666
Tensile Strength, Ultimate 440 MPa63800 psi
Tensile Strength, Yield 400 MPa58000 psi
Elongation at Break 4.0 %4.0 %In 50 mm
Modulus of Elasticity 115 GPa16700 ksi
Poissons Ratio 0.3070.307
Machinability 20 %20 %UNS C36000 (free-cutting brass) = 100%
Shear Modulus 44.0 GPa6380 ksi
Shear Strength 275 MPa39900 psi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity  0.00000244 ohm-cm
@Temperature 1100 °C
0.00000244 ohm-cm
@Temperature 2010 °F
liquid phase
 0.00000310 ohm-cm
@Temperature 20.0 °C
0.00000310 ohm-cm
@Temperature 68.0 °F
annealed
Magnetic Susceptibility -0.0000125 - -1.00e-6-0.0000125 - -1.00e-6SI units
 
Thermal PropertiesMetricEnglishComments
CTE, linear 18.0 µm/m-°C
@Temperature 20.0 - 300 °C
10.0 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.380 J/g-°C0.0908 BTU/lb-°F
Thermal Conductivity 234 W/m-K
@Temperature 20.0 °C
1620 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
Melting Point 1050 - 1065 °C1920 - 1949 °F
Solidus 1050 °C1920 °F
Liquidus 1065 °C1949 °F
 
Processing PropertiesMetricEnglishComments
Annealing Temperature 425 - 800 °C797 - 1470 °F
Hot-Working Temperature 750 - 875 °C1380 - 1610 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 94 - 96 %94 - 96 %
Iron, Fe <= 0.050 %<= 0.050 %
Lead, Pb <= 0.050 %<= 0.050 %
Zinc, Zn 5.0 %5.0 %
 
Descriptive Properties
Velocity of Sound3.78 km/sat 20°C

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Cartridge Brass, UNS C26000 (260 Brass), H08 Temper flat products
Commercial Bronze, UNS C22000 (90-10 Bronze), H08 Temper flat products
Gilding Copper, UNS C21000, Quarter Hard Temper
Gilding Copper, UNS C21000, Extra Hard Temper
Overview of materials for Brass

MC21000b9 / 10986

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.