MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
LCY ValuPrene p-TPV 65A BK Thermoplastic Vulcanized Elastomers
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: A medium hardness, black color, multi-purpose thermoplastic elastomer featuring good compression set and moderate temperature performance. ValuPrene 65A BK can be processed by extrusion for applications such as weatherstrip profile, seals, and window gaskets.

Attributes:

  • ValuPrene p-TPV is designed for applications requiring sealing performance at moderate temperatures.
  • Suitable for profile extrusion.
  • Conventional thermoplastic processing equipment can be used.
Applications: ValuPrene p-TPV has good sealing property, chemical, weathering resistance and electrical property that is suitable for TPV, thermoset EPDM rubber, Styrene based TPE, flexible PVC and other TPE applications. It is a good choice for applications requiring flexibility in the following markets: automotive parts, appliance, construction, consumer products, and electronics.

Information provided by LCY Chemical Corp.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.960 g/ccISO 1183
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 68
@Time 15.0 sec
Injection Molded; ISO 868
Tensile Strength at Break 10.0 MPa500 mm/min; ISO 37
Elongation at Break 700 %500 mm/min; ISO 37
100% Modulus 2.50 MPa500 mm/min; ISO 37
Tear Strength 26.0 kN/m500 mm/min; ISO 34-1
Compression Set 21 %
@Temperature 23.0 °C,
Time 79200 sec
ISO 815
 42 %
@Temperature 77.0 °C,
Time 79200 sec
ISO 815
 
Thermal PropertiesOriginal ValueComments
Melting Point 150 °C
 
Processing PropertiesOriginal ValueComments
Zone 1 170 °CExtrusion
Zone 2 180 °CExtrusion
Zone 3 190 °CExtrusion
Zone 4 200 °CExtrusion
Zone 5 210 °CExtrusion
Die Temperature 210 °CExtrusion
Melt Temperature 170 - 210 °CExtrusion
Roll Temperature 20.0 - 50.0 °CExtrusion
Shelf Life 36.0 Month
 
Descriptive Properties
Screen Pack20-60 meshExtrusion
Screw> 20:1 (Typical 24:1)Screw L/D ratio, General Purpose
 2.5~3 : 1Compression ratio

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLCY134 / 295677

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.