MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Glyptal G6332 Gloss Enamel
Categories: Polymer; Thermoset; Epoxy; Epoxy Cure Resin

Material Notes: GLYPTAL 6332 green gloss enamel is a specially-developed, durable enamel for finishing apparatus to be stored or operated outdoors. Equally suitable for indoor use. May be used on metal or wood.

Information provided by Glyptal Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.971 g/cc0.0351 lb/in³
Solids Content 37 %37 %Volume
 50 %50 %Weight
Thickness >= 25.4 microns>= 1.00 milDry Film
 
Optical PropertiesMetricEnglishComments
Gloss >= 80 %>= 80 %60°
 
Processing PropertiesMetricEnglishComments
Tack-Free Time 240 min4.00 hour
 
Descriptive Properties
Adhesion1Cross Hatch
ColorGreen
MethodSpray or brush
ReducerMineral spiritsFor brush
 XyleneFor spray
Solvent SystemXyleneClean-up
SubstrateSteel
Viscosity70-78 KU

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PGLYPT931 / 209770

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.