MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Okulen® OKULEN® PP B – natural – FN0000 PP B
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: OKULEN® PP B is a natural basic stabilization polypropylene blockcopolymer with high melt viscosity and good low-temperature impact strength.

Properties: Good chemical resistance; High heat deflection temperature; Easy to work and weld

Color: Natural FN0000

Range of applications: Punching pads

Information provided by Okulen

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.901 g/cc0.0326 lb/in³DIN EN ISO 11831-1
Water Absorption <= 0.010 %<= 0.010 %DIN EN ISO 62
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 72 - 74
@Time 3.00 sec
72 - 74
@Time 0.000833 hour
6 mm plate; DIN EN ISO 868
Tensile Strength, Yield >= 25.0 MPa>= 3630 psi1B- 50 mm/min; DIN EN ISO 527-2
Tensile Modulus >= 1.20 GPa>= 174 ksi1B- 1 mm/min; DIN EN ISO 527-2
Izod Impact, Notched (ISO) >= 20.0 kJ/m²>= 9.52 ft-lb/in²DIN EN ISO 21304-2
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cmDIN EN 62631-3-1
Surface Resistance >= 1.00e+15 ohm>= 1.00e+15 ohmDIN EN 62631-3-2
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 15.0 - 20.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
8.33 - 11.1 µin/in-°F
@Temperature 73.4 - 176 °F
ISO 11359
Thermal Conductivity 0.220 W/m-K1.53 BTU-in/hr-ft²-°F
Melting Point 158 - 165 °C316 - 329 °FDIN EN ISO 11357-1
Flammability, UL94 HBHB
 
Descriptive Properties
Operation Temperature100°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

POKUL1050 / 307327

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.