MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
DuPont Selar® PA 2072 Nylon Barrier Resin
Categories: Polymer; Film; Thermoplastic; Nylon (Polyamide PA); Nylon, Barrier Film Copolymer

Material Notes: Selar® PA 2072 is an amorphous nylon (polyamide) resin which is specially designed for blending with ethylene vinyl alcohol (EVOH) copolymers. Selar® PA 2072 can be tumble-blended with most grades of EVOH to form blends which combine the excellent barrier properties of EVOH with the deep-draw thermoforming properties, processing flexibility and moisture-insensitivity of Selar® PA. In addition, Selar® PA 2072 provides better adhesion in blends with EVOH than other grades of amorphous nylon, and this may allow converters to use less expensive adhesives.

Information provided by DuPont Packaging Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.19 g/ccASTM D1505
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 70.0 MPaASTM D882
Film Elongation at Break, MD 20 %Orientation not specified; ASTM D882
Flexural Modulus 2.80 GPaat 50% RH; ASTM D790
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 125 °CASTM D3418
 
Optical PropertiesOriginal ValueComments
Haze <= 1.0 %ASTM D1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DuPont Selar® PA 3426 Nylon Barrier Resin
Dow Surlyn® 1650SB
DuPont™ Selar® PA 3426R Nylon Barrier Resin
Dow Bynel® 50E803 Anhydride Modified Polypropylene
Dow Bynel® 50E806 Anhydride Modified Polypropylene

PDUPL1 / 33657

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.