This product is part of a range of Heat Curable Inks designed specifically for use in Electro Luminescent systems. Phosphor Inks containing these polymers combine excellent chemical, environmental with good flexibility to ITO. This polymeric binder is offered as a raw Material to those customers wishing to compound their own phosphor inks. Screen Printing Equipment: semi-automatic, manual Screen Types: stainless steel, polyester Substrate: ITO coated polyesterInformation provided by Gwent Electronic Materials Ltd. |