MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
LyondellBasell Koattro DP 8510M Plastomer  (discontinued **)
Categories: Polymer; Thermoplastic; Polybutene

Material Notes: Koattro is a novel family of high-molecular-weight plastomers. Polybutene-1 grade Koattro DP8510M is a random copolymer of butene-1 with high ethylene content. This product is primarily used in hot melt adhesive formulations and to improve rheological properties in blends. Koattro DP8510M is highly compatible with polypropylene due to its similar structure but less compatible in blends with polyethylene, but still easily dispersible. Its relatively slow kinetics of crystallization allow for an excellent wetting behavior. Its high shear-sensitive flow behavior means that it remains easily dispersible also in even more incompatible polymers like thermoplastic elastomers. Applications: Coatings, Protective, Hot Melt Adhesives, Hygiene Nonwoven, Specialty Film.

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.897 g/ccISO 1183-1
Melt Flow 40 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133-1
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 25.0 MPaISO 8986-2
Elongation at Break 300 %ISO 8986-2
Flexural Modulus 120 MPaISO 178
 
Thermal PropertiesOriginal ValueComments
Melting Point 81.0 °CTm2; ISO 11357-3
 94.0 °CTm1; ISO 11357-3
 
Descriptive Properties
Processing MethodContinuous Filament/Spinning, Fibers, Spunbond, Staple Fiber

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEQT7600 / 219237

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.