MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

ExxonMobil Enmist EP 220
Categories: Fluid; Lubricant

Material Notes: Esso ENMIST EP is a family of premium quality industrial lubricants designed for the oil-fog or mist-lubrication of machine components such as slideways, bearings, gears, chains etc. ENMIST EP mist lubricants are formulated with base stocks carefully selected for outstanding low-temperature properties and a proprietary additive package for exceptional stray mist control and oxidation stability. The outstanding oxidation stability of ENMIST EP resists deposit formation under high-temperature operating conditions, which helps reduce wear rates and extend equipment life. Their low pour points reduce the risk of wax plugging at the reclassifier, which could otherwise cause premature equipment failure, particularly in dry sump applications. The formulation of ENMIST EP is carefully balanced to ensure that the additives do not severely reduce the oil-to-air ratio in the oil-mist system, which might prevent adequate lubrication of the machine elements. ENMIST EP is fortified with anti-wear and EP agents that provide highly effective protection, especially for heavily loaded bearings and gears, such as those used in the metal rolling industry. The advanced, proprietary, technology of Esso ENMIST EP has been proven in field and laboratory tests to lubricate and protect equipment over a wide range of operating temperatures and conditions. Use of Esso ENMIST EP can reduce overall costs by reducing premature bearing and gear failures, cutting repair costs, and extending equipment life. Its low-stray-mist tendencies can significantly improve the quality of the work environment and enhance safety. Care should be taken to use ENMIST EP in accordance with the viscosity-temperature recommendations of the equipment manufacturer. ENMIST EP oils are available in five viscosity grades from ISO VG 100 to 460.

Esso ENMIST EP oils are designed for use in all oil mist lubrication systems. Such systems work by dispersing very small droplets of oil in smoothly flowing air, distributing the oil mist to the points of application and mechanically condensing the mist, causing the oil to impinge on and wet the surfaces to be lubricated. The higher viscosity Esso ENMIST EP grades may require thermal misting devices to form proper dispersions when ambient temperatures are moderate or low. Esso ENMIST EP provides dependable performance in the oil-mist lubrication systems of major manufacturers such as Alemite, Bijur, Lubrication Systems Company, Norgren, Trabon and others. It is also suitable for oil/air systems. Specific applications include: Industrial gearing such as cooling tower gearboxes; Slow-speed, heavily-loaded bearings; Machine tools, ways and screws; Process pumps, electric motors and blowers; Steam turbines

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity Measurement 7373Index; ASTM D2270
Kinematic Viscosity at 40°C (104°F) 220 cSt220 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 16.5 cSt16.5 cStASTM D445
 
Thermal PropertiesMetricEnglishComments
Pour Point -22.0 °C-7.60 °FASTM D97
Flash Point 222 °C432 °FASTM D92
 
Descriptive Properties
Rust Prevention, Synthetic Sea WaterpassASTM D665B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WEXXON243 / 75668

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.