MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

ITW Insulcast® LN 1-05 Epoxy Potting/Encapsulation Compound
Categories: Polymer; Thermoset; Epoxy

Material Notes: Insulcast® solutions are compounds designed for potting and encapsulating. INSULCAST LN 1-05 is a non-cracking epoxy compound that was specifically designed for large potting and encapsulation applications. It displays excellent electrical properties over a wide range of temperatures. INSULCAST LN 1-05 makes use of the latest polymer and filler technology.

Information provided by ITW Performance Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.940 g/cc0.940 g/ccUncured. Part B
 1.62 g/cc1.62 g/ccUncured. Part A
Viscosity 10 cP10 cPUncured. Part B; ASTM D2393
 5000 cP5000 cPUncured, mixed; ASTM D2393
 120000 cP120000 cPPart A; ASTM D2393
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8585ASTM D2240
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 6.00e+15 ohm-cm6.00e+15 ohm-cmASTM D257
Dielectric Constant 5.15
@Frequency 1000 Hz
5.15
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 15.7 kV/mm400 kV/inASTM D149
Dissipation Factor 0.010
@Frequency 1000 Hz
0.010
@Frequency 1000 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear 32.0 µm/m-°C17.8 µin/in-°F
Thermal Conductivity 0.648 W/m-K4.50 BTU-in/hr-ft²-°F
 0.648 W/m-K4.50 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 105 °C221 °F
Minimum Service Temperature, Air -40.0 °C-40.0 °F
Glass Transition Temp, Tg 72.0 - 78.0 °C162 - 172 °F
Flammability, UL94 V-0V-0
 
Processing PropertiesMetricEnglishComments
Pot Life 8.00 - 10.0 min8.00 - 10.0 minPart A
 8.00 - 10.0 min8.00 - 10.0 minPart B
Shelf Life 12.0 Month12.0 MonthPart B
 12.0 Month12.0 MonthPart A
 
Descriptive Properties
ColorBlackUncured. Part A
 NeutralUncured. Part B
Mix Ratio by volume4.15:1Part A: Part B
Mix Ratio by weight7.2:1Part A: Part B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PITWIN9093 / 239603

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.