MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Park Aerospace Nelcote® E-766B Epoxy Prepreg, 7581 E-Glass Reinforced
Categories: Polymer; Thermoset; Epoxy

Material Notes: Nelcote® E-766B is a low tack, self adhesive epoxy resin system designed for honeycomb applications. E-766B displays excellent peel properties.

Key Features and Benefits:

  • Self adhesive resin system for sandwich panel applications
  • Flame retardant and self-extinguishing
  • Low tack and long out-times for ease of processing

Applications/Qualifications:

  • Sandwich panels / structures
  • Aircraft Interiors
  • Mass Transit Interiors

Information provided by Park Electrochemical Corp.

Key Words: EP
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Volatiles <= 1.0 %
@Temperature 163 °C
<= 1.0 %
@Temperature 325 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 448 MPa
@Temperature 23.9 °C
65000 psi
@Temperature 75.0 °F
ASTM D3039
Tensile Modulus 21.4 GPa
@Temperature 23.9 °C
3100 ksi
@Temperature 75.0 °F
Dry; ASTM D3039
Compressive Strength 448 MPa
@Temperature 23.9 °C
65000 psi
@Temperature 75.0 °F
Dry; ASTM D695
Compressive Modulus 22.1 GPa
@Temperature 23.9 °C
3200 ksi
@Temperature 75.0 °F
Dry; ASTM D695
Shear Strength 53.8 MPa
@Temperature 23.9 °C
7800 psi
@Temperature 75.0 °F
Short-Beam, Dry; ASTM D2344
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 93.0 °C199 °FDry; DMA
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month
@Temperature -17.8 °C
12.0 Month
@Temperature 0.000 °F
 
Descriptive Properties
Fabric Area Weight (g/m²)300
Prepreg Resin Content (%)37-43
Resin Flow (%)15-21275°F, 15psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Hexcel® HexForce™ 7581 Fiber Glass Fabric
Hexcel® HexPly® M26/M26T 120°C (250°F) Curing Epoxy Matrix, M26T/50%/7581 Glass Fabric

PPARK040 / 89312

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.