MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

SABIC LNP™ THERMOCOMP™ KF002L Acetal (Asia)  (Unverified Data**)
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Homopolymer, Glass Fiber Reinforced

Material Notes: LNP THERMOCOMP KF002L is a compound based on Acetal Homopolymer resin containing 10% Glass Fiber. Added features of this material include: Low Extractible.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.49 g/cc0.0538 lb/in³ASTM D792
 1.49 g/cc0.0538 lb/in³ISO 1183
Moisture Absorption 0.200 %0.200 %50% RH, 24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.016 - 0.018 cm/cm0.016 - 0.018 in/in24 hrs; ASTM D955
 0.017 cm/cm0.017 in/in24 hrs; ISO 294
Linear Mold Shrinkage, Transverse 0.015 - 0.017 cm/cm0.015 - 0.017 in/in24 hrs; ASTM D955
 0.016 cm/cm0.016 in/in24 hrs; ISO 294
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 63.0 MPa9140 psiASTM D638
 63.0 MPa9140 psiISO 527
Tensile Strength, Yield 65.0 MPa9430 psiISO 527
 66.0 MPa9570 psiASTM D638
Elongation at Break 3.2 %3.2 %ISO 527
 3.4 %3.4 %ASTM D638
Elongation at Yield 2.1 %2.1 %ISO 527
 2.2 %2.2 %ASTM D638
Flexural Strength 103 MPa14900 psiASTM D790
 105 MPa15200 psiISO 178
Flexural Modulus 4.40 GPa638 ksiISO 178
 4.82 GPa699 ksiISO 178/1A
Izod Impact, Notched 0.420 J/cm0.787 ft-lb/inASTM D256
Izod Impact, Unnotched 3.84 J/cm7.19 ft-lb/inASTM D4812
Izod Impact, Notched (ISO) 4.00 kJ/m²1.90 ft-lb/in²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 26.0 kJ/m²12.4 ft-lb/in²80*10*4; ISO 180/1U
Impact Test 2.00 J1.48 ft-lbMultiaxial Impact; ISO 6603
Instrumented Impact Energy at Peak 6.00 J4.43 ft-lbASTM D3763
Tangent Modulus 5600 MPa812000 psi1 mm/min; ISO 527
 6200 MPa899000 psi50 mm/min; ASTM D638
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  10.8 µm/m-°C
@Temperature -40.0 - 40.0 °C
6.00 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E 831
 112 µm/m-°C
@Temperature -40.0 - 40.0 °C
62.2 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow  5.40 µm/m-°C
@Temperature -40.0 - 40.0 °C
3.00 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E 831
 60.5 µm/m-°C
@Temperature -40.0 - 40.0 °C
33.6 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 162 °C324 °FFlatw 80*10*4 sp=64mm; ISO 75/Bf
 162 °C
@Thickness 3.20 mm
324 °F
@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 148 °C298 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 155 °C
@Thickness 3.20 mm
311 °F
@Thickness 0.126 in
unannealed; ASTM D648
 
Processing PropertiesMetricEnglishComments
Zone 1 175 - 190 °C347 - 374 °F
Zone 2 195 - 205 °C383 - 401 °F
Zone 3 210 - 220 °C410 - 428 °F
Melt Temperature 200 - 215 °C392 - 419 °F
Mold Temperature 80.0 - 110 °C176 - 230 °F
Drying Temperature 80.0 °C176 °F
Dry Time 4.00 hour4.00 hour
Back Pressure 0.200 - 0.300 MPa29.0 - 43.5 psi
Screw Speed 30 - 60 rpm30 - 60 rpm

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultraform® H 2320 006 Q600 POM
Owens Corning Glass Fiber Reinforced Acetal, 25 wt.% glass
DuPont Mobility and Materials Delrin® 500PE BK602 POM
Delrin Delrin® 520MP NC010 POM-SD20
Delrin Delrin® 500P BK602 POM

PSABI21158 / 214294

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.