MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Spartech Royalite R57 FR/ABS Aircraft Grade Sheet
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Sheet

Material Notes: Description: Aircraft Grade Sheet

Information provided by Spartech.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.18 - 1.26 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 93ASTM D785
Tensile Strength, Yield 5000 psiASTM D638
Flexural Yield Strength 7800 psiASTM D790
Flexural Modulus 280000 psiASTM D790
Izod Impact, Notched 9.00 ft-lb/in73°F; ASTM D256
 1.60 ft-lb/in
@Temperature -28.9 °C
ASTM D256
Instrumented Impact Total Energy 30.0 ft-lb
@Temperature 22.8 °C
Dynatup Instrumented Impact; ASTM D3763
 
Thermal PropertiesOriginal ValueComments
CTE, linear 46.0 - 55.0 µin/in-°F
@Temperature 20.0 °C
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 172 °FASTM D648
 
Descriptive Properties
FAA 12 Second Vertical BurnPassesFAR Pt 25, App F, Pt I
FlammabilityPasses MVSS (Motor Vehicle Safety Standard) 302

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Polymer Resources ABS-FR Flame Retardant ABS
Spartech Royalite R570 FR-ABS Fire Rated Sheet
Spartech Korad® SP-9071 FR/ABS Flame Retardant Sheet
Spartech SP-9013 FR/ABS Flame Retardant Sheet
PTS Trilac® ABS-HS6500 High Impact ABS Resin

PROY49 / 66409

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.