CYROLITE® Protect and CYROLITE® Protect 2 acrylic-based multipolymer compounds and CYREX® Protect acrylic-polycarbonate alloy provide antimicrobial capabilities* against a variety of microorganisms commonly found in healthcare facilities. Antimicrobial products are used in medical devices for secondary infection management or to inhibit bacterial growth. Benefits: - Antimicrobial capabilities within the polymer structure. No secondary operations required.
- Chemical resistance to lipids and alcohol
- Easily welded
- Bondable to PVC tubing
- Excellent impact strength
- EtO, gamma and e-beam sterilizable
Transparent blue tint, free of bisphenol A (BPA), superior resistance to lipids and alcohol as well as excellent ductilityThe former Cyro/Evonik Methacrylates business has been sold to Röhm (Roehm) GmbH. |