MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ravago Manufacturing Americas Hylon® N1035HHR BK Nylon 66, 35% Glass Fiber Reinforced, Heat Stabilized, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 40% Glass Fiber Filled; Nylon 66, Heat Stabilized

Material Notes: Product Description: PA 66, 35% Glass Fiber Reinforced, Heat Stabilized, Lubricated, Heat/Hydrolysis Resistant, Black Color

Availability: North America

Filler/Reinforcement: Glass Fiber, 35% Filler by Weight

Additive: Heat Stabilizer; Lubricant

Features: Good Heat Resistance; Heat Stabilized; Hydrolysis Resistant; Lubricated

RoSH Compliance: RoSH Compliant

Automotive Specifications: CHRYSLER MS-DB-41 CPN2727 Color: Black; FORD WSK-M4D752-A Color: Black

Appearance: Black

Information provided by Ravago Manufacturing Americas

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.38 g/cc0.0499 lb/in³ISO 1183
Water Absorption 0.70 %
@Time 86400 sec
0.70 %
@Time 24.0 hour
ISO 62
Linear Mold Shrinkage, Flow 0.0030 - 0.0050 cm/cm
@Thickness 3.17 mm
0.0030 - 0.0050 in/in
@Thickness 0.125 in
ISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 178 MPa25800 psiISO 527-2
Elongation at Break 2.0 %2.0 %ISO 527-2
Flexural Strength 275 MPa39900 psiISO 178
Flexural Modulus 9.79 GPa1420 ksiISO 178
Izod Impact, Notched (ISO) 10.1 kJ/m²4.80 ft-lb/in²ISO 180
Charpy Impact, Notched 1.01 J/cm²4.80 ft-lb/in²ISO 179
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 255 °C491 °FUnannealed; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 243 °C469 °FUnannealed; ISO 75-2/A

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PRAVAGO4973 / 311666

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.