MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Envalior ForTii® Eco LDS62B PA*-GF35 PA4T High Temperature Polyamide
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Nylon (Polyamide PA)

Material Notes: ForTii® is a high temperature polyamide for applications in the electronics, lighting, automotive, white goods, industrial and aerospace industries.

ForTii® Eco LDS62B is a high ductility LDS material which enables good structural integrity in complicated geometries. It is well suited for wearable devices and smart phone antennas for consumer electronics. It has excellent dimensional stability to ensure low warpage after chemical plating. Eco LDS62B is Eco-friendly due to its partly bio-based content. Features: Bio-based - 14C measurable. Laser Direct Structuring. Low warpage. 35% glass reinforced. Processing: Injection molding.

Former DSM Engineering Plastics product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.50 g/ccDry; ISO 1183
Linear Mold Shrinkage, Flow 0.0021 cm/cmDry; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0070 cm/cmDry; ISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 130 MPaDry; ISO 527-1/-2
Elongation at Break 1.7 %Dry; ISO 527-1/-2
Tensile Modulus 11500 MPaDry; ISO 527-1/-2
Flexural Strength 190 MPaDry; ISO 178
Flexural Modulus 10000 MPaDry; ISO 178
Charpy Impact, Notched 4.60 kJ/m²
@Temperature 23.0 °C
Dry; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 3.74
@Frequency 1e+9 Hz
Dry; IEC 60250
 3.8
@Frequency 1e+9 Hz
Cond; IEC 60250
 
Thermal PropertiesOriginal ValueComments
CTE, linear 66.0 µm/m-°CDry; ISO 11359-1/-2
CTE, linear, Parallel to Flow 17.0 µm/m-°CDry; ISO 11359-1/-2
Melting Point 319 °C10°C/min. Dry; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 235 °CDry; ISO 75-1/-2
Flammability, UL94 HB
@Thickness 1.50 mm
Dry; IEC 60695-11-10
 HB
@Thickness 3.00 mm
Dry; IEC 60695-11-10

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDSM7929 / 291365

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.