MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Apcotex Apcoflex® P3380 4C NBR Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Description: Apcoflex® P3380 4C is a medium Acrylonitrile, very high Mooney Viscosity pre-crosslinked rubber in powdered form. It is partitioned with Calcium Carbonate.

Applications: Apcoflex® P3380 4C powder is recommended for the modification of PVC in Injection Moulded and Extruded Goods. It is also used in the manufacture of PVC based TPEs. P3380 4C also finds application in Asbestos and non-asbestos Gaskets, Brake liners and brake pads in automotive and railways. The addition of Apcoflex Powders helps in improving abrasion resistance and reducing noise in these products.

CAS No: 9003-18-3

Information provided by Apcotex Industries Limited

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Volatiles <= 0.70 %<= 0.70 %
Mooney Viscosity 75 - 90
@Temperature 100 °C
75 - 90
@Temperature 212 °F
ML 1+4
Ash 5.0 - 9.0 %5.0 - 9.0 %
Storage Temperature <= 35.0 °C<= 95.0 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life <= 12.0 Month<= 12.0 Month
 
Descriptive Properties
Content32-35%Bound Acrylonitrile (Polymer)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PAPCOT026 / 315605

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.