MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Alfa Chemistry Materials Polydimethyl Siloxane, dihydroxy terminated, MW 110000
Material Notes: Silicone OH polymer is colorless clear liquid, with most properties of dimethylsilicone fluid, besides it also of the hydroxy reaction activity.

Applications: It is mainly used to produce paint additives, rubber additives, textile additives

Molecular Formula: HO[-Si(CH3)2O-] nH

Synonyms: SILICON PS 347.5;SILANOL TERMINATED POLYDIMETHYLSILOXANE;SILANOL TERMINATED POLYDIMETHYLSILOXANE,18000CS;SILANOL TERMINATED POLYDIMETHYLSILOXANES;PS 347.5;POLYDIMETHYLSILOXANE, DIHYDROXY TERMINATED;POLYDIMETHYLSILOXANE, SILANOL TERMINATED;baysilonc0.7

Alfa Chemistry Materials product group: Polymer/Macromolecule

Manufacturer data sheet

Vendors: Alfa Chemistry is an ISO 9001:2015 certified supplier of various materials, including: MOFs, coatings, nanomaterials, metals, polymers, carbon fibers, graphite, ceramics, glass, semiconductors, catalysts, carbon nanotubes, fullerene, COFs, molecular sieve, quantum dots, recycled plastics, photonic and optical materials, and magnetic materials, for customers worldwide. Alfa Chemistry also provides custom synthesis services for nearly all kinds of materials and chemicals. Learn more about Alfa Chemistry's high quality products at materials.alfachemic.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 0.975 g/cc
@Temperature 20.0 °C
0.0352 lb/in³
@Temperature 68.0 °F
Viscosity Measure 50000 cSt50000 cSt
Molecular Weight 110000 g/mol110000 g/mol
 
Thermal PropertiesMetricEnglishComments
Boiling Point >= 204 °C>= 399 °F
Flash Point 338 °C640 °F
 
Descriptive Properties
CAS Number70131-67-8

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

ZZALFA68414 / 304585

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.