MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
ExxonMobil Santoprene® 123-50W175 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: A hard, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in thin wall applications. This grade of Santoprene TPV is shear-dependent and can be processed on conventional thermoplastics equipment for injection molding, extrusion or blow molding. It is polyolefin based and completely recyclable.

Key Features:

  • Recommended for applications requiring excellent flex fatigue resistance.
  • Recommended for applications requiring excellent ozone resistance.
  • Designed for improved UV resistance.
  • EU and China RoHS compliant
Applications:
  • Automotive- Seals, Gaskets and Weather Seals
Uses:
  • Automotive Applications
  • Automotive Exterior Trim
Availability: Africa & Middle East, Europe, North America, Asia Pacific, Latin America and South America

Information provided by ExxonMobil Chemical

Key Words: EU 2003/11/EC; RoHS Compliant
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.950 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 51
@Thickness 2.00 mm,
Time 15.0 sec
ISO 868
Tensile Strength, Yield 1640 psiAcross Flow; ASTM D638
Elongation at Break 32 %Across Flow; ASTM D638
 
Processing PropertiesOriginal ValueComments
Processing Temperature 175 - 230 °C
 
Descriptive Properties
Change in Mass in IRM 903 Oil at 257°F for 70 hr99
ColorBlack
FormPellets

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Zylog Neoplast® 173 C Thermoplastic Vulcanizate
Multibase TPSiV® 1180-50D Thermoplastic Silicone Vulcanizate
ExxonMobil Santoprene® 273-50 Thermoplastic Elastomer

PADVA077 / 22767

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.