MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Americhem Engineered Compounds ColorFast® FRPS200 Styrene, High Impact
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Flame Retardant; Polystyrene, Impact Modified

Material Notes: V0/5VA high impact styrene

All information provided by LTL Color Compounders, Inc. LTL was acquired by Americhem in 2014.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.15 g/cc1.15 g/ccASTM D792
Linear Mold Shrinkage 0.0030 - 0.0060 cm/cm0.0030 - 0.0060 in/in0.125 in.; ASTM D955
Melt Flow 6.5 g/10 min
@Load 5.00 kg,
Temperature 200 °C
6.5 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell L 6161ASTM D785
Tensile Strength at Break 24.8 MPa3600 psi2.0 in/min; ASTM D638
Tensile Strength, Yield 24.1 MPa3500 psi2.0 in/min; ASTM D638
Elongation at Break 35 %35 %2.0 in/min; ASTM D638
Flexural Modulus 2.00 GPa290 ksi2.0 in/min; ASTM D790
Izod Impact, Notched 0.961 J/cm
@Temperature 22.8 °C
1.80 ft-lb/in
@Temperature 73.0 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 86.1 °C187 °FUnannealed (0.250"); ASTM D648
Flammability, UL94 V-0V-0
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 171 - 199 °C340 - 390 °F
Middle Barrel Temperature 193 - 227 °C380 - 440 °F
Front Barrel Temperature 218 - 254 °C425 - 490 °F
Nozzle Temperature 204 - 232 °C400 - 450 °F
Melt Temperature 204 - 238 °C400 - 460 °F
Mold Temperature 10.0 - 71.1 °C50.0 - 160 °F
Drying Temperature 71.1 °C160 °F
Dry Time 2 - 4 hour2 - 4 hournominal; maximum drying time of 8 hours
Back Pressure 0.345 - 0.689 MPa50.0 - 100 psi
Shot Size 40 - 60 %40 - 60 %
Vent Depth 0.00254 - 0.00762 cm0.00100 - 0.00300 in
Screw Speed 40 - 70 rpm40 - 70 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLTLC034 / 104419

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.