MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Neodymium, Nd
Categories: Metal; Nonferrous Metal; Pure Element

Material Notes: Silver Metal; Hexagonal

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 7.01 g/cc0.253 lb/in³
 
Chemical PropertiesMetricEnglishComments
Atomic Mass 144.24144.241995
Atomic Number 6060
X-ray Absorption Edge 0.28451 Å0.28451 ÅK
 1.73759 Å1.73759 ÅLI
 1.84244 Å1.84244 ÅLII
 1.99452 Å1.99452 ÅLIII
Electronegativity 1.141.14Pauling
Ionic Radius 0.995 Å0.995 ÅCrystal Ionic Radius for Valence +3
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 1818
Tensile Strength, Ultimate 170 MPa24700 psi
Tensile Strength, Yield 165 MPa23900 psi
Elongation at Break 25 %25 %
Modulus of Elasticity 41.4 GPa6000 ksi
Bulk Modulus 31.8 GPa4610 ksi
Poissons Ratio 0.2810.281
Shear Modulus 16.3 GPa2360 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000643 ohm-cm0.0000643 ohm-cm
Magnetic Susceptibility 0.00003920.0000392cgs/g
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 49.3 J/g21.2 BTU/lb
CTE, linear 9.60 µm/m-°C
@Temperature 20.0 °C
5.33 µin/in-°F
@Temperature 68.0 °F
Specific Heat Capacity 0.153 J/g-°C0.0366 BTU/lb-°FGas
 0.190 J/g-°C0.0454 BTU/lb-°F
Thermal Conductivity 13.0 W/m-K90.2 BTU-in/hr-ft²-°F
Melting Point 1010 °C1850 °F
Boiling Point 3074 °C5565 °F
Heat of Formation 0.000 kJ/mol0.000 kJ/molCrystal
 327.6 kJ/mol327.6 kJ/molGas
 
Optical PropertiesMetricEnglishComments
Emissivity (0-1) 0.394
@Wavelength >=645 nm,
Temperature 1021 - 1567 °C
0.394
@Wavelength >=645 nm,
Temperature 1870 - 2853 °F
liquid total hemispherical
 
Component Elements PropertiesMetricEnglishComments
Neodymium, Nd 100 %100 %
 
Descriptive Properties
CAS Number7440-00-8

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Alliance N-42 Neodymium Iron Boron Magnetic Material
Alliance N-33 Neodymium Iron Boron Magnetic Material
Silver, Ag
Aluminum, Al
Nickel, Ni

AMENd00 / 69

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.