MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
General Industrial Polymers ANIONIC LATEX LTX 5A Styrene-Butadiene Copolymer Latex
Categories: Polymer; Thermoplastic; Styrene-Butadiene; Styrene-Butadiene Copolymer, SBC

Material Notes: Latex LTX 5A is a cold polymerized, high solids styrene-butadiene copolymer latex stabilized with a fatty acid emulsifier.

Applications:
Latex Mastic Adhesives consists of a group of high solids lattices with a proven track record of over 40 years of success in adhesives. The high molecular weight of the Latex LTX 5A provides adhesives with excellent cohesive strength. This coupled with early leg development makes it an excellent choice for flooring adhesives and an added plus for the installer.
SBR Latex for Asphalt Modification High solids SBR latex products have been used as modifiers in asphalt materials for more than 30 years and have been found to provide several improvements in the asphalt roads. These improvements include resistance to high temperature permanent deformation, resistance to cold temperature cracking, and an improvement in short and long term aging. High and low molecular weight SBR latices are available to provide the required balance between compatibility and reinforcement for a given asphalt material.
Latex Foam Products SBR High Solids Latices are an ideal choice for your latex foam application. Latex LTX 5A is the work horse rubber latex and the product of choice if you seek high resiliency in your gel and non-gel foam applications.

Information provided by General Industrail Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 68.5 - 71 %
Particle Mesh Size 80 Mesh<0.1%, Coagulum
pH 9.8 - 10.5
Brookfield Viscosity 1200 - 2000 cP
Mooney Viscosity 100 - 160ML-4’
Surface Tension 31 - 35 dynes/cm
 
Chemical PropertiesOriginal ValueComments
Styrene Content 22.5 - 25 %Bound
 
Descriptive Properties
Content<200 ppmResidual Styrene
 4.5-6.2%Soap Content

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PGENIND009 / 294798

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.