MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

ConocoPhillips Hydroclear® 68 2 EP gear Oil
Categories: Fluid; Lubricant

Material Notes: Conoco Hydroclear EP Gear Oil is a premium extreme-pressure industrial gear lubricant with superior deposit control. Hydroclear EP Gear Oil is formulated with proprietary additive chemistry and Conoco premium oils hydrocracked base oil. It is recommended for use in severe service enclosed-gear sets. Hydroclear EP Gear Oil provides “clean gear” performance with exceptional oxidation inhibition, EP load-carrying capacity, foam control, rust and corrosion protection and rapid low-temperature demulsibility. Hydroclear EP Gear Oil is capable of extending intervals between oil changes by providing “clean gear” performance, coupled with superior oxidation control. Hydroclear EP Gear Oil significantly exceeds the requirements of and has been formally approved by Cincinnati Milacron in accordance with its Lubricant Specifications (ISO 68 to 460, respectively – P-63, 76, 77, 74, 59 and 35). Hydroclear EP Gear Oil exceeds AGMA Specification 9005 (replacement for 250.04) and U.S. Steel 224 Specification for enclosed-gear lubricants.

Information provided by ConocoPhillips.

Phillips 66 Lubricants was spun-off from ConocoPhillips in 2012, and branding was further reorganized in 2016. The Hydroclear® trade name is no longer in use but products may be available under different names.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.874 g/cc0.0316 lb/in³
Viscosity Measurement 9898Viscosity Index
Saybolt Viscosity at 100°F 374 SUS374 SUS
Saybolt Viscosity at 210°F 56 SUS56 SUS
Kinematic Viscosity at 40°C (104°F) 72 cSt72 cSt
Kinematic Viscosity at 100°C (212°F) 8.7 cSt8.7 cSt
ASTM Color 2.52.5
 
Mechanical PropertiesMetricEnglishComments
Four Ball Extreme Pressure, Weld Load 250 kg551 lb (mass)
Four Ball Wear 0.300 mm0.0118 in
Timken Test 31700 g70.0 lb
 
Thermal PropertiesMetricEnglishComments
Pour Point -34.4 °C-30.0 °F
Flash Point 235 °C455 °F
 
Descriptive Properties
Corrosion, Copper Strip1B
Demulsibility, Emulsion0ASTM D2711
Demulsibility, Free Water85ASTM D2711
Demulsibility, Water in Oil0.6ASTM D2711
Emulsion Characteristics (40-40-0)15 minutes
Foam Control (Sequence I,II,III)0-0-0
FZGPass 12 Load Stages
Oxidation Control 1.2 % vis. increaseASTM D2893

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WCON084 / 75121

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.