MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Total HT 514 MDPE film
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Film Grade

Material Notes: Finathene® HT 514 is a medium density polyethylene produced by the slurry loop low pressure polymerization process.

Finathene® HT 514 can be used alone, blended or coextruded in a wide variety of blown film applications : liquid food, fat food, freezer, heavy duty, shrink hoods, liners, refuse, carriers, produce, labels, protective, mulch, diapers, .

Information provided provided by Total Petrochemicals.

Total Petrochemicals acquired former Fina and Atofina plastics product lines.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.938 g/cc0.0339 lb/in³ASTM D 792
Melt Flow  0.15 g/10 min
@Load 2.16 kg
0.15 g/10 min
@Load 4.76 lb
ASTM D 1238
 0.80 g/10 min
@Load 5.00 kg
0.80 g/10 min
@Load 11.0 lb
ASTM D 1238
High Load Melt Index 14 g/10 min
@Load 21.6 kg
14 g/10 min
@Load 47.6 lb
ASTM D 1238
 
Mechanical PropertiesMetricEnglishComments
Dart Drop Test 80.0 g0.176 lb40µm film, LDPE
 >= 130 g>= 0.287 lb20µm film, HDPE
 
Descriptive Properties
Food StatusFormulated to comply with most requirements of food packaging regulations

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Braskem HF 0150 HDPE Blown Film Extrusion Polyethylene
Reliance Industries Relene E52009 Polyethylene
Total Lacqtene® 6002 FLG 42 HDPE film
Dow ELITE™ 5400G Enhanced Polyethylene Resin
Dow AFFINITY™ PL 1881G Polyolefin Plastomer (POP)

PFINAP102 / 38685

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.