MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

NuSil EPM-2421 Silicone, Potting & Encapsulating Material
Categories: Polymer; Thermoset; Silicone

Material Notes: General Purpose: Potting & Encapulating Materials

Comments: Low Viscosity, Self-leveling, General Adhesive and Encapsulant

Cure system: Platinum

Information provided by NuSil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.02 g/cc1.02 g/cc
Viscosity 2700 cP2700 cPB
 3750 cP3750 cPA
 
Chemical PropertiesMetricEnglishComments
Ionic Impurities - Na (Sodium) <= 4.0 ppm<= 4.0 ppm
Ionic Impurities - K (Potassium) <= 2.0 ppm<= 2.0 ppm
Ionic Impurities - Cl (Chloride) <= 5.0 ppm<= 5.0 ppm
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 5050
Tensile Strength at Break 5.50 MPa798 psi
Elongation at Break 90 %90 %
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmASTM D257
Dielectric Strength 21.7 kV/mm550 kV/inASTM D149
 
Processing PropertiesMetricEnglishComments
Cure Time 15.0 min
@Temperature 150 °C
0.250 hour
@Temperature 302 °F
Working Life 180 min
@Temperature 25.0 °C
180 min
@Temperature 77.0 °F
 
Descriptive Properties
ColorClear
Mix Ratio1:1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
NuSil CV15-2500 Silicone, Two Part Adhesive and Sealant

PNUSIL253 / 141977

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.