MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

(Viewing data as-entered. Click here to return)
Arkema Rilsamid® AESNO MED Nylon 12
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12)

Material Notes: Rilsamid® AESNO MED is a rigid polyamide 12 with high viscosity designed for tube extrusion. This grade dedicated to extrusion offers the highest quality and it is specifically designed to meet the stringent requirements of the medical applications such as minimally invasive devices. Upon request letters regarding USP Class VI compliance can be provided. Designation: PA12, EHL, 22-010

Information provided by Arkema.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.01 g/ccISO 1183
Water Absorption 1.6 %Dry; Sim. to ISO 62
Melt Flow 8.0 g/10 min
@Load 5.00 kg,
Temperature 235 °C
cm³/10 min Volumetric Rate; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Puncture Resistance 4800 N
@Temperature -30.0 °C
Maximum Force, Cond.; ISO 6603-2
Tensile Strength, Yield 43.0 MPaCond.; ISO 527-1/-2
 50.0 MPaDry; ISO 527-1/-2
Elongation at Break >= 50 %Dry; ISO 527-1/-2
 >= 50 %Cond.; ISO 527-1/-2
Elongation at Yield 5.0 %Dry; ISO 527-1/-2
 5.0 %Cond.; ISO 527-1/-2
Tensile Modulus 1440 MPaCond.; ISO 527-1/-2
 1500 MPaDry; ISO 527-1/-2
Charpy Impact Unnotched NB
@Temperature -30.0 °C
Cond.; ISO 179/1eU
 NB
@Temperature 23.0 °C
Cond.; ISO 179/1eU
Charpy Impact, Notched 6.00 kJ/m²
@Temperature -30.0 °C
Cond.; ISO 179/1eA
 11.0 kJ/m²
@Temperature 23.0 °C
Cond.; ISO 179/1eA
Puncture Energy 60.0 J
@Temperature -30.0 °C
Cond.; ISO 6603-2
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+14 ohm-cmCond.; IEC 60093
Surface Resistance 1.00e+14 ohmCond.; IEC 60093
Dielectric Strength 30.0 kV/mmCond.; IEC 60243-1
Comparative Tracking Index 600 VCond.; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 100 µm/m-°CDry; ISO 11359-1/-2
Melting Point 180 °C10°C/min; Dry; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 135 °CDry; ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °CDry; ISO 75-1/-2
Vicat Softening Point 142 °C50°C/h 50N; Dry; ISO 306
 
Descriptive Properties
Form as DeliveredPellets
Moisture SensitiveYes
Processing MethodsFilm Extrusion
 Other Extrusion
 Profile Extrusion
 Sheet Extrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Arkema Rilsan® BESNO MED Nylon 11
W. L. Gore GORE™ 800 PTFE Universal Pipe Gasket (Style 800)
Evonik Vestamid® L2140 Nylon 12
Arkema Pebax® 3533 SA 01 MED Polyether Block Amide (PEBA)
Arkema Pebax® 7233 SA 01 MED Polyether Block Amide (PEBA)

PARKG675d / 142951

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.