MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Polyram Polytron P30N07 Polypropylene, 30% Long Glass Fiber, UV Stabilized
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 30% Glass Fiber Filler

Material Notes: A chemically coupled 30% LGF reinforced natural PP, heat stabilized, UV stabilized for injection molding applications.

Information provided by Polyram.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.12 g/ccISO 1183
Linear Mold Shrinkage 0.0017 cm/cmISO 2577
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 100 MPaISO 527
Elongation at Break 2.6 %ISO 527
Tensile Modulus 6000 MPaISO 527
Flexural Strength 150 MPaISO 178
Flexural Modulus 5200 MPaISO 178
Izod Impact, Notched (ISO) 18.0 kJ/m²ISO 180
Charpy Impact Unnotched 60.0 kJ/m²ISO 179
Charpy Impact, Notched 18.0 kJ/m²ISO 179
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 149 °CISO 75
Flammability, UL94 HB
@Thickness 3.00 mm
Glow Wire Flammability Index 750 °CIEC 60695

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
PlastiComp Complet® LCF30 - PP Homopolymer Polypropylene, 30% Long Carbon Fiber Reinforced
Westlake Plastics Propylux® CN-F Polypropylene (conductive)
RTP Company RTP 181 HI  Polypropylene (PP) Carbon Fiber 10% - High Impact
RTP Company RTP 1081 Polybutylene Terephthalate (PBT), Carbon Fiber
Celanese SO.F.TER Carboprene® 2530AV Talc-Reinforced Polypropylene

PPOLYR944 / 126741

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.