MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Henkel Loctite® Stycast® 1090 SI CAT 11 Two-Component Epoxy
Categories: Polymer; Thermoset; Epoxy; Epoxy Encapsulant, Unreinforced

Material Notes: Product Benefits

  • Low density
  • Low dielectric constant
  • Two component
  • Low viscosity
  • Low cure shrinkage
  • Low CTE
  • Long pot life
  • Excellent chemical resistance
  • Excellent physical and chemical properties at elevated temperatures

Cure: Heat Cure

Application: Encapsulation

Loctite Stycast 1090 SI CAT 11 is designed for encapsulation and potting of electronic assemblies that require lower weight such as aerospace applications. It is completely unicellular so moisture absorption is negligible.

Loctite Stycast 1090 SI can be used with a variety of catalysts. For more information on mixed properties when used with other available catalysts, please contact your local technical service representative for assistance and recommendations

Information provided by Henkel.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.700 g/ccPart A, Loctite Stycast 1090 SI
Density 0.700 g/ccMixed
Water Absorption 0.13 %Cured; ASTM D570
Viscosity 3500 cPMixed
 35 - 60 cP
@Temperature 65.0 °C
Part B, Loctite CAT 11
Brookfield Viscosity 40000 cPPart A, Loctite Stycast 1090 SI; 10 rpm, #6
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 80ISO 868
Tensile Strength 37.0 MPaISO 37
Flexural Strength 50.0 MPaASTM D790
Compressive Strength 83.0 MPaISO 604
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+13 ohm-cmIEC 60093
Dielectric Constant 2.3
@Frequency 1e+6 Hz
Dissipation Factor 0.030
@Frequency 1e+6 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 43.0 µm/m-°CASTM D3386
Thermal Conductivity 0.170 W/m-K
Maximum Service Temperature, Air 155 °C
Minimum Service Temperature, Air -55.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 0.500 - 1.00 hour
@Temperature 120 °C
Option 3, Post Cure: 2 to 4 hours at the highest expected use temperature
 2.00 - 4.00 hour
@Temperature 100 °C
Option 2, Post Cure: 2 to 4 hours at the highest expected use temperature
 8.00 - 16.0 hour
@Temperature 80.0 °C
Option 1, Post Cure: 2 to 4 hours at the highest expected use temperature
Working Life >= 240 min
@Temperature 25.0 °C
100 g mass
Shelf Life 12.0 MonthPart A, Loctite Stycast 1090 SI
 
Descriptive Properties
AppearanceBlackPart A, Loctite Stycast 1090 SI
Mix Ratio, by Volume100 : 8Resin : Hardener
Mix Ratio, by Weight100 : 13.5Resin : Hardener

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHENK7909 / 255396

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.