MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Cabot CAB-O-SILĀ® TS-720 Fumed Silica
Categories: Other Engineering Material

Material Notes: CAB-O-SIL TS-720 fumed silica is a medium surface area fumed silica which has been surface treated with polydimethylsiloxane (PDMS). This surface treatment results in a hydrophobic silica with a very different performance than untreated silica. CAB-O-SIL TS-720 fumed silica is characterized by:
  • Thickening efficiency
  • Sag resistance or high film build
  • Anti-settling of pigments and fillers
  • Stable rheological performance over time
Key applications: CAB-O-SIL TS-720 fumed silica is used for rheology control in a wide variety of adhesives, composite and coatings applications. This product provides the following performance advantages in medium to high polarity systems:
  • Thickening efficiency
  • Sag resistance or high film build
  • Anti-settling of pigments and fillers
  • Shear-thinning rheological behavior
  • Stable rheological performance over time
Epoxy Adhesives and Coatings: In epoxy adhesives and coatings, CAB-O-SIL TS-720 fumed silica provides good thickening efficiency, sag resistance (or film build) and anti-settling of pigments and fillers.
Polyurethane Adhesives and Coatings: In polyurethane adhesives and coatings, CAB-O-SIL TS-720 fumed silica provides the same efficient, stable rheology control as in epoxy systems. In addition, the hydrophobic surface of CAB-O-SIL TS-720 fumed silica introduces very little moisture into these systems, retarding premature cross-linking of moisture cured systems.
Vinyl Ester Laminating Resins and Gel Coats: While untreated silicas are effective thickeners of unsaturated polyester resins, CAB-O-SIL TS-720 fumed silica is a more efficient, stable rheology control additive for higher polarity systems like vinyl ester laminating resins and gel coats.

Information provided by Cabot Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Descriptive Properties
Product FormPowder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCABOT101 / 315836

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.