MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
GEHR Plastics PEEK Polyetheretherketone
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK)

Material Notes: Polyether etherketone can be used at very high temperatures and it shows good mechanical strength, toughness, hardness, flexural strength, and torsional strength. PEEK exhibits excellent chemical resistance, very good dielectric properties up to 260°C and a very good resistance to all kinds of radiation.

Properties:

  • very high mechanical strength
  • very high rigidity
  • very high thermal stability
  • very high creep resistance
  • very high dimensional stability
  • very high radiation resistance
  • very high hydrolysis resistance
  • relatively low notch impact-strength
  • low resistance against acetone
Applications include bearing shells, piston rings, valve seats, gears, seals, aviation, cog-wheels, pump vanes, fittings, plug connectors, and wafer carriers.

Vendors: Ensinger TECAPEEK™ shapes are manufactured exclusively with Victrex™ PEEK polymer. The Ensinger process and Victrex resins ensure reliability, consistency, dimensional stability, and high temperature mechanical performance.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.32 g/ccISO 1183
Moisture Absorption at Equilibrium 0.070 %ISO 62
Water Absorption at Saturation 0.40 %ISO 62
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 99ISO 2039
Hardness, Shore D 90ISO 868
Ball Indentation Hardness 250 MPaISO 2039
Tensile Strength at Break 67.0 MPaISO 527
Tensile Strength, Yield 91.0 MPaISO 527
Elongation at Break 11 %ISO 527
Elongation at Yield 7.0 %ISO 527
Modulus of Elasticity 4.21 GPaISO 527
Flexural Strength 170 MPaISO 178
Charpy Impact Unnotched NBISO 179
Charpy Impact, Notched 4.00 kJ/m²ISO 179
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 3.00e+13 ohm-cmIEC 60093
Surface Resistance >= 1.00e+13 ohmIEC 60093
Dielectric Constant 3.2
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 16.0 kV/mmIEC 60243-1
Dielectric Loss Index 0.0030
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 125 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear 47.0 µm/m-°CISO 11359
Thermal Conductivity 0.250 W/m-K
@Temperature 20.0 °C
ISO 22007-4
Melting Point 340 °CDIN EN ISO 3146
Maximum Service Temperature, Air 260 °CUL 746B
Deflection Temperature at 0.46 MPa (66 psi) 240 °CISO 75
Deflection Temperature at 1.8 MPa (264 psi) 158 °CISO 75
Vicat Softening Point 250 °CVST/B/50; ISO 306
Minimum Service Temperature, Air -40.0 °CUL 746B
Glass Transition Temp, Tg 143 °CDIN EN ISO 3146
Flammability, UL94 V-0UL 94
Oxygen Index 35 %ASTM D2863
 
Compliance PropertiesOriginal ValueComments
FDA YesPhysiological indifference
 
Descriptive Properties
Acid Resistanceyes
Aromatic Resistanceyes
Bondabilityyes
CKW Resistancelimited
Colornatural
Hydrocarbonate Resistanceyes
Hydroxide Resistanceyes
Ketone Resistanceyes
Physiological indifferenceyes, EEC
Resistance Against Hot Wateryes
UV Stabilizationlimited

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Polyetheretherketone, Unreinforced
E-Glass Fiber, Generic
Mitsubishi Chemical Advanced Materials Ketron™ 1000 PEEK, Extruded Unfilled Polyetherether Ketone
Ensinger Tecapeek® Polyetheretherketone (PEEK)
Celanese VECTRA E150i LCP, 50% Glass Reinforced

PGEHR037 / 79874

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.