MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Dover Chemical DOVERNOX 3114 Tris isocyanurate
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Dovernox 3114 is a high purity, non-discoloring, non-staining high molecular weight hindered phenol antioxidant. It exhibits low volatility and low extractability in film, fiber, and mineral filled polypropylene applications. Use levels can range from 0.10 to 0.50%

Information provided by DoverChem

Key Words: CAS# 27676-62-6
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solubility in Water 0.010 %
@Temperature 20.0 °C
0.010 %
@Temperature 68.0 °F
Solubility  2000 ppm
@Temperature 20.0 °C
2000 ppm
@Temperature 68.0 °F
Hexane
 >= 5000 ppm
@Temperature 20.0 °C
>= 5000 ppm
@Temperature 68.0 °F
Methanol
 270000 ppm
@Temperature 20.0 °C
270000 ppm
@Temperature 68.0 °F
Acetone
 320000 ppm
@Temperature 20.0 °C
320000 ppm
@Temperature 68.0 °F
Ethyl Acetate
Molecular Weight 784 g/mol784 g/mol
 
Thermal PropertiesMetricEnglishComments
Melting Point 218 °C424 °F
 
Descriptive Properties
Physical FormWhite Free Flowing Powder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Evonik ROHAMERE® 6878-O Ethoxylated Bisphenol A-Dimethacrylate (Liquid)

WDOVER024 / 217643

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.