MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Henkel Turco 5578-L Etchant
Categories: Fluid; Solvent

Material Notes: Turco 5578-L is an amber, liquid compound formulated to clean and etch titanium, columbium and tantalum alloys by spray or immersion systems. Readily removes mill soils, marking inks, lube oils, cutting oil and fingerprints at a low concentration, and will etch titanium at higher concentrations. It is an effective etch prior to adhesive bonding, diffusion bonding, painting, welding and brazing.
    Applications:
  • Alkaline Etch
  • Alkaline Cleaning

Key Words: Aerospace Surface Treatment
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Descriptive Properties
ChemistryStrong Alkaline
ConsistencyLiquid
FormConcentrated
SubstrateTitanium

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI 4130 Steel, annealed at 865°C (1585°F), furnace cooled 11°C (20°F)/hour to 680°C (1255°F), air cooled, 25 mm (1 in.) round
H.C. Starck Amperit® 599.074 Agglomerated Sintered Molybdenum Carbide (Cr2O3)
CuMoCu 13/74/13
Cabot 10 Tantalum Alloy (UNS R05255)
ASTM A182, Grade F11, Class 2

PHENK894 / 146899

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.