MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Beijing Evergrow Resources UHMW PE Fiber Rope
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); UHMW PE (Ultra High Molecular Weight PE)

Material Notes:

Information provided by Beijing Evergrow Resources.

Key Words: UHMWPE, PE
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Descriptive Properties
Lay12
Tenacity (ton)1012mm Diameter
 1816mm Diameter
 2420mm Diameter
 2822mm Diameter
 36mm Diameter
 3525mm Diameter
 4828mm Diameter
 5630mm Diameter
 8038mm Diameter
 8640mm Diameter
Weight per Length (kg/100m)1616mm Diameter
 2.56mm Diameter
 2520mm Diameter
 2922mm Diameter
 3825mm Diameter
 5028mm Diameter
 5430mm Diameter
 8.512mm Diameter
 8138mm Diameter
 8840mm Diameter

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Beijing Evergrow Resources UHF-R2400 UHMW PE Fiber
Industeel SOLEIL A2 13% Cr High Strength Martensitic Stainless Steel (QT550 Heat Treatment)
Westlake Plastics LenniteĀ® Biocompatible Implant Grade UHMW-PE
410 Stainless Steel
Overview of materials for Low Density Polyethylene (LDPE), Molded

PBEIJ022 / 90091

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.