MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company RTP 381 EM Polycarbonate (PC), Carbon Fiber - Easy Molding - Self Extinguishing - Halogen Free - UL94 V-2
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Carbon Fiber Reinforced

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.22 g/cc1.22 g/ccASTM D 792
Filler Content 10 %10 %Primary Additive
Water Absorption 0.12 %0.12 %24 hrs @ 23°C; ASTM D 570
Linear Mold Shrinkage 0.00050 - 0.0020 cm/cm
@Thickness 3.17 mm
0.00050 - 0.0020 in/in
@Thickness 0.125 in
ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 117 MPa17000 psiASTM D 638
Elongation at Break 2.5 - 3.5 %2.5 - 3.5 %ASTM D 638
Tensile Modulus 7.58 GPa1100 ksiASTM D 638
Flexural Strength 179 MPa26000 psiASTM D 790
Flexural Modulus 6.89 GPa1000 ksiASTM D 790
Izod Impact, Notched 1.07 J/cm
@Thickness 3.17 mm
2.00 ft-lb/in
@Thickness 0.125 in
D 256
Izod Impact, Unnotched 5.87 J/cm
@Thickness 3.17 mm
11.0 ft-lb/in
@Thickness 0.125 in
ASTM D4812
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity <= 1e+05<= 1e+05ASTM D 257
Surface Resistivity per Square <= 1.00e+6 ohm<= 1.00e+6 ohmASTM D 257
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 146 °C295 °FASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 141 °C285 °FASTM D 648
Flammability, UL94  V-2
@Thickness 1.59 mm
V-2
@Thickness 0.0625 in
 V-0
@Thickness 3.17 mm
V-0
@Thickness 0.125 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 288 - 316 °C550 - 600 °F
Mold Temperature 82.2 - 121 °C180 - 250 °F
Drying Temperature 121 °C250 °F
Dry Time 4 hour4 hour
Moisture Content 0.020 %0.020 %
Dew Point -28.9 °C-20.0 °F
Injection Pressure 68.9 - 103 MPa10000 - 15000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
PTS Tristar® PC-10FRNH-V 12 MFI Non-Bromine Non-Chlorine Flame Retardant UV Stabilized Polycarbonate With Release
PTS Tristar® PC-10FR 12 MFI Flame Retardant Polycarbonate With Release
Mitsubishi Xantar® MX 1081 Polycarbonate-10% Glass Reinforced
Mitsubishi Iupilon® ECF 2010R Polycarbonate

PQZWA1180 / 90652

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.