MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

High Conductivity Bronze, UNS C40500, H08 Temper flat products
Categories: Metal; Nonferrous Metal; Copper Alloy; Bronze

Material Notes: Good to excellent corrosion resistance. Excellent cold workability. Fabricated by blanking, forming and drawing.

Applications: meter clips, terminals, fuse clips, contact and relay springs, washers.

Test specimen: flat products - 1mm thickness.

Key Words: Copper, penny bronze
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.83 g/cc0.319 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 7979
Hardness, Rockwell 30T 7171
Tensile Strength, Ultimate 510 MPa74000 psi
Tensile Strength, Yield  435 MPa
@Strain 0.5 %
63100 psi
@Strain 0.5 %
 495 MPa
@Strain 0.2 %
71800 psi
@Strain 0.2 %
Elongation at Break 4.0 %4.0 %In 50 mm
Modulus of Elasticity 110 GPa16000 ksiHard
 125 GPa18100 ksiAnnealed
Machinability 20 %20 %UNS C36000 (free-cutting brass) = 100%
Shear Strength 295 MPa42800 psi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000420 ohm-cm0.00000420 ohm-cm
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 165 W/m-K
@Temperature 20.0 °C
1150 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
Melting Point 1025 - 1060 °C1877 - 1940 °F
Solidus 1025 °C1877 °F
Liquidus 1060 °C1940 °F
 
Processing PropertiesMetricEnglishComments
Annealing Temperature 510 - 670 °C950 - 1240 °F
Hot-Working Temperature 830 - 890 °C1530 - 1630 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 95 %95 %
Tin, Sn 1.0 %1.0 %
Zinc, Zn 4.0 %4.0 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Phosphor bronze 1.25% Sn, UNS C50500, OSO75 Temper, 0.015 mm Grain Size
High Conductivity Bronze, UNS C40500, OSO15 Temper flat products
High Conductivity Bronze, UNS C40500, H10 Temper flat products
High Conductivity Bronze, UNS C40500, H06 Temper flat products
High Conductivity Bronze, UNS C40500, H04 Temper flat products

MC40500c1 / 11264

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.