MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Lushan L-5R (F) Polyethylene Copolymer Adhesive for Steel Pipe Coating
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Copolymer adhesive resin Lushan L-5R series is maleic anhydride grafted polyethylene which could be in granule or powder form. It was developed by Lushan with independent patent technologies and proved with excellent performance in the widely applications of pipeline projects both in China and international market. The purpose of the adhesive is to bond the epoxy layer to the top coat. Copolymer adhesive resin Lushan L-5R series in mainly used as adhesive layer in 3 layers polyethylene system (3LPE) for steel pipe against corrosion coating system in oil and gas pipeline and high pressure water pipeline. Copolymer adhesive resin Lushan L-5R series has good properties such as high bonding strength, long-term stability, wide compatibility, easy processing, etc. Copolymer adhesive resin Lushan L-5R series designed to meet with requirements of the following National and international standards, under the condition that appropriate industrial processing method are applied under a continuous quality control system and when used in combination copolymer adhesive resin Lushan L-5R& polyethylene compound top coats EJ-1 and compatible powder epoxy.

Information provided by Lushan

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.945 g/ccASTM D792
Carbon Black Loading >= 2.0 %ASTM D1603
Melt Flow >= 0.17 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
 1.5 - 2.5 g/10 min
@Load 5.00 kg,
Temperature 190 °C
ISO 1133
Melt Index of Compound 6.0 g/10 minASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 23.0 MPaASTM D638
Elongation at Break 800 %ASTM D638
Peel Strength >= 120 kN/m50+5°C; ISO 21809-1
 >= 160 kN/m20+5°C; ISO 21809-1
 
Thermal PropertiesOriginal ValueComments
Melting Point 134 °CASTM D2117
Maximum Service Temperature, Air 60.0 °C
Vicat Softening Point 113 °CASTM D1525
Minimum Service Temperature, Air -40.0 °C
Brittleness Temperature -70.0 °CASTM D746
 
Descriptive Properties
Appearancegranule

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lushan L-5R (HC) Polyethylene Copolymer Adhesive for Steel Pipe Coating

PLUSH003 / 150001

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.