MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

3M XG5110 General Purpose Double Coated Tape
Categories: Polymer; Adhesive

Material Notes: 3M™ X-Series Industrial Attachment Tapes offer a variety of performance characteristics and product construction to support demanding application requirements. This product line provides a range of adhesive transfer and double-coated tapes designed for attachment of paper, corrugated, films, foils, fabric plastics and metal. Double Coated (DC) tapes provide a backing for improved handling. Adhesive Transfer Tapes (ATT) provide the thinnest bold lines. The 3M™ X-Series Tape System is manufactured in the United States by 3M.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 76.2 microns3.00 milRelease Liner
 102 microns4.00 milTape
 
Mechanical PropertiesMetricEnglishComments
Peel Strength 0.789 kN/m4.50 pliFaceside, to Stainless Steel, 180° Peel, 2 mil Al
 0.84363 kN/m4.8125 pliBackside, to Stainless Steel, 180° Peel, 2 mil Al
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 65.0 °C149 °FLong Term
 82.0 °C180 °FShort Term
 
Processing PropertiesMetricEnglishComments
Shelf Life 18.0 Month18.0 Month
 
Descriptive Properties
Adhesive CarrierPolyester Film
Adhesive TypeGeneral Purpose Acrylic
LinerWhite Densified Kraft Liner with Red Print

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMM33969 / 168716

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.