Usual surface texture: Coarse Dimensional changes when dried lumber is subjected to variations in humidity during service: Medium Resistance to fungal decay (Heartwood in ground contact): Moderately Durable (10 to 15 years) Resistance to penetration by preservatives: Moderately resistant Common Applications: Structural work, turnery, joinery, furniture |
Pometia Pinnata; Lumber, Timber |