MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
DuPont Surlyn® PC2000  (discontinued **)
Categories: Polymer; Thermoplastic; Ethylene Methyl Acrylate

Material Notes: DuPont™ Surlyn® PC2000 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with sodium ions. The high MAA content and mid-range neutralization level for this grade creates an exceptional combination of strengths: toughness, low-temperature toughness, abrasion resistance, tear resistance, excellent clarity, and high stiffness compared with other grades of Surlyn®. The resin is highly suitable for injection molding, providing enhanced processability over other grades. Surlyn ® PC2000 is ideal for applications where easy melt flow characteristics and high stiffness, high clarity and good abrasion resistance are desired. In golf ball covers, it provides good cut resistance, impact durability, high resiliency and increased coefficient of restitution, particularly when used in blends with different cations.

Information provided by DuPont™

This product line/trade name was acquired by Dow, but this specific grade was discontinued prior to the acquisition.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.970 g/ccASTM D792-ISO 1183
Melt Flow 4.5 g/10 min
@Load 2.16 kg
Condition E; ASTM D1238, ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 65ASTM D2240-ISO 868
Tensile Strength at Break 4496 psiASTM D638 ISO 527-2
Tensile Strength, Yield 2698 psiASTM D638
Elongation at Break 320 %ASTM D638 ISO 527-2
Flexural Modulus 0.490 GPaASTM D790
Tensile Impact Strength 427 ft-lb/in²ASTM D1822
Abrasion 301NBS Index; ASTM D1630
 
Thermal PropertiesOriginal ValueComments
Melting Point 104 °CFreezing Point; ASTM D3418
 183 °CASTM D3417- ISO 3146
Vicat Softening Point 127 °CASTM D1525, ISO 306
 
Optical PropertiesOriginal ValueComments
Haze 1.3 %ASTM D1003

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow Nucrel® 0411HS Ethylene-Methacrylic Acid Copolymer Resin for Extrusion Coating/Laminating
INEOS Styrolution NAS® 30 Styrene Methyl Methacrylate (SMMA)
Arkema LOTRYL® Bestpeel 2407 Copolymer Ethylene - Methyl Acrylate
Arkema LOTRYL® 29 MA 03 Copolymer Ethylene - Methyl Acrylate
Arkema LOTRYL® 28 MA 07 Copolymer Ethylene - Methyl Acrylate

PDUP955 / 33522

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.