MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Epoxies, Etc 20-3236 Elastomer Modified Epoxy for Vinyl Adhesion
Categories: Polymer; Thermoset; Epoxy

Material Notes: Description: 20-3236 Resin is a low viscosity copolymer adhesive and potting compound specifically designed for bonding vinyls and neoprenes. 20-3236 Resin has an extended working time and a convenient 2:1 mix ratio. 20-3236 Resin can be used in many difficult bonding applications. It is also used for the encapsulation of vinyl insulated electrical components or sealing vinyl lead wires.

Features:

  • Bonds to vinyls and neoprenes
  • Long working time
  • Low viscosity
  • High peel strength

Information provided by Epoxies, Etc

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.07 g/cccatalyzed
Water Absorption 0.21 %
@Time 86400 sec
Viscosity 3000 cPMixed
Storage Temperature 40.0 - 60.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 80
Tensile Strength 8300 psi
Elongation at Break 6.4 %
Izod Impact, Notched 0.550 ft-lb/in
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 9.00e+16 ohm-cm
Dielectric Constant 3.57
@Frequency 1e+6 Hz
Dissipation Factor 0.021
@Frequency 1e+6 Hz
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 120 °C
Minimum Service Temperature, Air -55.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 2.00 - 3.00 hour
@Temperature 65.0 °C
 6.00 - 8.00 hour
@Temperature 45.0 °C
 24.0 - 36.0 hour
@Temperature 25.0 °C
Pot Life 300 min
@Load 0.100 kg
Shelf Life 6.00 Month
 
Descriptive Properties
ColorAmber

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PFEPOX035 / 316712

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.