MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ThyssenKrupp XAR® PLUS Structural Steel
Categories: Metal; Ferrous Metal; Carbon Steel; Low Carbon Steel

Material Notes: This Material Specification applies to 3 to 100 mm thick plates of the wear-resistant special structural steel XAR® PLUS.

Application: The steel may be used for wear exposed structures, e.g. excavating, mining and earth-moving machinery, truck dump bodies, conveying, crushing and pulverizing equipment, scrap presses and paving moulds.

Information Provided by Thyssen Krupp

Key Words: EN 1.8722
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 1350 MPa
Tensile Strength, Yield 1200 MPa
Elongation at Break 10 %
Charpy Impact 30.0 J
@Temperature -40.0 °C
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al <= 1.3 %
Boron, B <= 0.0050 %
Carbon, C <= 0.22 %
Chromium, Cr <= 1.3 %
Copper, Cu <= 0.30 %
Iron, Fe >= 93.5 %As Balance
Manganese, Mn <= 1.5 %
Molybdenum, Mo <= 0.50 %
Other <= 0.55 %Carbon Equivalent
Phosphorus, P <= 0.025 %
Silicon, Si <= 0.80 %
Sulfur, S <= 0.012 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Special Metals Nitinol High-Strength Superelastic Ni-Ti alloy
SAE J2477 AD 1600 Automotive Austempered Ductile Iron
Overview - Alumina, 96%, Al2O3
Niobium Carbide, NbC
NanoAmor 50% Regular Single Walled Carbon Nanotubes

NTHYSS031 / 90351

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.