MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Chemical Concepts Chem-Set™ Stone Tac Aerosol Low Bloom Accelerator
Categories: Polymer; Adhesive; Thermoset

Material Notes: Chem-Set™ Stone Tac will aid the bonding of porous materials such as fabrics or woods. It is useful when bonding acidic surfaces or in low humidity conditions promoting consistent curing times. Ideal for wire tacking, silk screening, or loudspeaker assembly. Using Chem-Set™ Stone Tac will enable the adhesive to fill gaps up to 0.20". Chem-Set™ Stone Tac can be applied by brushing or spraying. Component in the Chem-Set™ CCA801 Chip Repair kit.

Information provided by Chemical Concepts™.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.760 g/ccQuick Tac 6
 0.790 g/ccQuick Tac 2
 0.790 g/ccQuick Tac 3
 0.790 g/ccQuick Tac 4
Viscosity 3.0 cPQuick Tac 2
 3.0 cPQuick Tac 3
 3.0 cPQuick Tac 4
 3.0 cPQuick Tac 5
 3.0 cPQuick Tac 6
 
Thermal PropertiesOriginal ValueComments
Boiling Point 133 °FQuick Tac 2
 154 °FQuick Tac 5
 180 - 181 °FQuick Tac 3
 >= 195 °FQuick Tac 4
 347 - 387 °FQuick Tac 6
Flash Point <= 0.000 °FQuick Tac 2
 15.0 °FQuick Tac 4
 53.0 °FQuick Tac 3
 120 °FQuick Tac 6
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 MonthQuick Tac 2, original sealed container when properly stored.
 12.0 MonthQuick Tac 3, original sealed container when properly stored.
 12.0 MonthQuick Tac 4, original sealed container when properly stored.
 12.0 MonthQuick Tac 5, original sealed container when properly stored.
 12.0 MonthQuick Tac 6, original sealed container when properly stored.
 
Descriptive Properties
ColorClear/Amber, Quick Tac 2
 Clear/Amber, Quick Tac 3
 Clear/Amber, Quick Tac 4
 Clear/Amber, Quick Tac 5
 Clear/Amber, Quick Tac 6
Solvent BaseAcetone, Quick Tac 2
 Heptane, Quick Tac 4
 Isopropanol, Quick Tac 3
 Mineral Spirits, Quick Tac 6
 N-Propyl Bromide, Quick Tac 5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCHEMI974 / 232171

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.