MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Kraiburg TPE THERMOLAST® K TF4CMB Thermoplastic Elastomer (FC/CM2 Series)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Styrenic TPE

Material Notes: The FC/CM2 series is a material solution for fatty food contact applications. It has an extremely low migration potential. The compounds are available in translucent and can be colored.

Processing Method: Injection Molding, Extrusion

Color / RAL DESIGN:

  • Translucent
Typical applications:
  • Packaging for food
  • Valves
  • Closures
  • Seals for housings
  • Household articles
  • Function and design elements
  • Membranes
  • Soft touch
Material advantages:
  • Optimized mechanical properties
  • Adhesion to PP
  • Colorable
  • In-process recycling possible
  • Low migration potential

Information provided by Kraiburg TPE

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³DIN EN ISO 1183-1
Storage Temperature 15.0 - 30.0 °C59.0 - 86.0 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 4040DIN ISO 48-4
Tensile Strength 11.0 MPa1600 psi200 mm/min; DIN 53504/ISO 37
Elongation at Break 900 %900 %200 mm/min; DIN 53504/ISO 37
Tear Strength 8.50 kN/m48.5 pliISO 34-1 Method B (b)
Compression Set 22 %
@Temperature 23.0 °C,
Time 259000 sec
22 %
@Temperature 73.4 °F,
Time 72.0 hour
DIN ISO 815-1 Method A
 
Descriptive Properties
ColorTranslucent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PKRAIA8194 / 308858

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.