MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Taiwan Sheen Soon Sheenthane® AS-120 TPU for PU Adhesive
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane TPE; Polyurethane, TP

Material Notes: Thermoplastic polyurethane elastomer for solvent-based polyurethane adhesive.

Max. toluene solubility, MC soluble

Excellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Used for footwear, textile laminations, furniture, spraying, and fire hose co-extrusion.

Information provided by Taiwan Sheen Soon Co., LTD.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity 70 - 130 cP15% solids in MEK
 
Mechanical PropertiesOriginal ValueComments
Peel Strength 0.170 - 0.340 kN/mInitial (5 min.) PVC vs. PVC
 
Descriptive Properties
Activation temperature (°C)55-65
Heat Resistance, mm6570°C, PVC vs PVC
Max. Toluene in Solvents (%)50-70
Tack Time, min15 ~ 25PVC vs PVC

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Taiwan Sheen Soon Sheenthane® AH-580 TPU for Hotmelt Adhesive
Taiwan Sheen Soon Sheenthane® AH-560 TPU for Hotmelt Adhesive
Taiwan Sheen Soon Sheenthane® AH-530 TPU for Hotmelt Adhesive
Taiwan Sheen Soon Sheenthane® AH-500 TPU for Hotmelt Adhesive
Taiwan Sheen Soon Sheenthane® AH-592 TPU for Hotmelt Adhesive

PSHEEN821 / 156225

Polyurethane

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.