Halogen-free, organically and inorganically filled melamine-modified Polyester molding compound. Low post-shrinkage, very good electrical values, high heat resistance, very good sliding behavior, very good wear stability. This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU directives 2002/95 (RoHS), 2002/96 (WEEE) and 2006/122 (PFOS) Processing: Injection and compression molding Applications: Molded parts in electrical engineering, mainly electrical parts such as circuit breakers, relays, switches, contact terminals. Information provided by the Raschig Group |