MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Alpha Nickel-Aluminum Bronze, UNS C95800, Copper Casting Alloy, M01 Temper, As Sand Cast
Categories: Metal; Nonferrous Metal; Copper Alloy; Bronze

Material Notes: Temper: As Sand Cast

Casting Characteristics: High – Drossing, Shrinkage in Solidification; Medium – Fluidity, Gassing; Low - Casting Yield, Effect of Section Size

Fabrication Properties: Excellent Suitability – Gas Shielded Arc Welding; Good Suitability – Soldering, Brazing, Coated Metal Arc Welding

Typical uses: Safety Tools; Nuts; Stator Clamps; Bushings; Gears; Hot Mill Guides; Impellers; Pickling Equipment; Propellers; Pump Casings; Stator Clamp Segments; Valves; Wear Plates; Welding Rods; Worms; Marine Hardware

Applicable Specifications: As Continuous Cast – ASTM B505/B505M; As Sand Cast – Castings ASTM B148; Ingot – ASTM B30

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.53 g/cc0.272 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 180
@Load 3000 kg
180
@Load 6610 lb
Tensile Strength >= 621 MPa>= 90000 psifor Standard
 655 MPa95000 psiTypical
Tensile Strength, Yield >= 276 MPa>= 40000 psifor Standard, 0.5% Ext
 310 MPa45000 psiTypical, 0.5% Ext
Elongation at Break >= 20 %>= 20 %for Standard
 26 %26 %Typical
Creep Strength 66.2 MPa9600 psi0.1% per 10,000 hours
Rupture Strength 234 MPa34000 psi
Tensile Modulus 124 GPa18000 ksi
Modulus of Rigidity 46.79 GPa6787 ksiCalculated
Compressive Strength 1030 MPa150000 psi0.1 in. set/in.
Poissons Ratio 0.3260.326
Fatigue Strength 228 MPa
@# of Cycles 1.00e+8
33000 psi
@# of Cycles 1.00e+8
Machinability 50 %50 %
Izod Impact 33.9 J25.0 ft-lb
Charpy Impact 40.7 J30.0 ft-lbV-Notch
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000570 ohm-cm0.0000570 ohm-cm3% IACS
Magnetic Permeability 1.031.03Annealed, Fast Cooled Condition
 2.22.2Slow Cooled Condition, Range 2.2 to 15.0
 
Thermal PropertiesMetricEnglishComments
CTE, linear 17.6 µm/m-°C
@Temperature 20.0 - 300 °C
9.80 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.439 J/g-°C0.105 BTU/lb-°F
Thermal Conductivity 1.01 W/m-K7.00 BTU-in/hr-ft²-°F
Melting Point 950.0 - 990.0 °C1742 - 1814 °F
Solidus 950.0 °C1742 °F
Liquidus 990.0 °C1814 °F
Shrinkage 1.56 %1.56 %Patternmaker's Shrinkage (3/16 in./ft.)
 
Processing PropertiesMetricEnglishComments
Processing Temperature 316 °C600 °FStress Relief
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 8.5 - 9.5 %8.5 - 9.5 %
Copper, Cu >= 79 %>= 79 %
Iron, Fe 3.5 - 4.5 %3.5 - 4.5 %should not exceed Ni content
Lead, Pb <= 0.03 %<= 0.03 %
Manganese, Mn 0.80 - 1.5 %0.80 - 1.5 %
Nickel, Ni 4.0 - 5.0 %4.0 - 5.0 %
Other, total <= 0.5 %<= 0.5 %
Silicon, Si <= 0.10 %<= 0.10 %
 
Descriptive Properties
Proportional Limit22 ksi
US EPA Registered AntimicrobialYes

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

MC95800x3 / 293248

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.