MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ChevronTexaco RPM® SAE 15W-40 Gas Engine Oil
Categories: Fluid; Lubricant

Material Notes: Features

Chevron RPM Gas Engine Oils is a premium quality heavy duty multigrade gas engine oil for use in engines running on compressed natural gas (CNG), liquefied natural gas (LNG), and liquefied petroleum gas (LPG).

It is formulated with Group II base stocks and a premium low ash additive package specially formulated for advanced lean burn, spark ignited, natural gas engines equipped with either roller or slider followers.

Chevron RPM Gas Engine Oil provides outstanding oxidation and nitration resistance, which reduce the buildup of insolubles and provide extended oil and filter life.

In vehicular and stationary four-stroke engines, Chevron RPM Gas Engine Oil:

  • minimizes valve recession
  • provides easier engine startup and better oil flow in low temperature conditions
  • reduces oil consumption

Applications

Chevron RPM Gas Engine Oil is recommended for these alternative fuel engines:

  • Cummins: B5.9G, C8.3G
  • Detroit Diesel: Series 50G, 60G
Chevron RPM Gas Engine Oil meets the performance requirements of:
  • Cummins: CES 20074 (B5.9G and C8.3G only)
  • Detroit Diesel: 7SE272-9510 (Series 50G and 60G only)
Chevron RPM Gas Engine Oil is recommended for use in slected alternative fuel vehicles – metropolitan transit vehicles and local delivery trucks operating on compressed natural gas (CNG), liquefied petroleum gas (LPG), or liquefied natural gas (LNG).

Key Words: CPS Number: 232344; MSDS Number: 8066
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
API Gravity 30.1 °
Viscosity 3150 cP
@Temperature -15.0 °C
Cold Crank
Viscosity Measurement 136Viscosity Index; ASTM D2270
Kinematic Viscosity at 40°C (104°F) 115 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 15 cStASTM D445
Ash 0.55 %Sulfated Ash wt%
 
Chemical PropertiesOriginal ValueComments
Total Base Number 5.1ASTM D2896
 
Thermal PropertiesOriginal ValueComments
Pour Point -36.0 °CASTM D97
Flash Point 230 °CASTM D92
 
Component Elements PropertiesOriginal ValueComments
Phosphorus, P 0.070 %
Zinc, Zn 0.078 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Sumitomo Bakelite Durez® 32341 Phenolic Resin
Sumitomo Bakelite Durez® 32340 Phenolic Resin
Rogers Arlon 23234R025 0.025" (0.635 mm) Semi-Cured Silicone Rubber with Fiberglass Substrate
Phillips 66 Trolley Wire Lube
Phillips 66 Kendall® Super-D® NG SAE Grade 15W-40

WCHEV069 / 74684

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.