Flexirene FF 25 is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for blown film extrusion. Flexirene FF 25 is characterized by a high elongational viscosity leading to a good bubble stability during extrusion. Main Applications: Flexirene FF 25 is recommended for the production of agriculture film, heavy duty bags, in blend or coextrusion with LDPE. Information provided by Polimeri Europa. Versalis is the Eni subsidiary containing the plastics and rubber businesses. |