- ISO 7391-PC,MFLR,(,,)-18-9
- Formerly Makrolon DP1-1872
- MVR (300 °C/1.2 kg) 19 cm3/10 min
- Flame retardant
- UL 94V-0/1.5 mm
- Low viscosity
- UV stabilized
- Easy release
- Injection molding - Melt temperature 280 - 320 °C
- Available in opaque colors only