MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Goodfellow Polyethylene Naphthalate (PEN) Film
Categories: Polymer; Film; Thermoplastic; Polyester, TP

Material Notes: A polyester that is chemically quite similar to PET but which is more temperature resistant. So far available only as biaxially oriented and heat stabilized films, they are semi-crystalline and colorless, either crystal clear or slightly hazy (the latter are available from Goodfellow stock). Compared to their PET equivalents, they start to shrink significantly at 190C rather than 150C and are certified for long term electrical use at 155C rather than 105/130C. Their tensile strengths are similar, but the modulus of PEN films is higher - say 25% at ambient temperatures but several times higher in the 100-150C region. They also have better UV resistance and barrier properties and are more resistant to hydrolysis in alkaline or very hot aqueous conditions. They are, however, more expensive and have a lower flex life.

Applications for the films are mainly in the electrical and electronic areas.

Information provided by Goodfellow.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.36 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 200 MPabiax film
Elongation at Break 60 %biax film
Tensile Modulus 5.00 - 5.50 GPabiax film
Coefficient of Friction 0.27biax film
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1.00e+15 ohm-cm
Surface Resistivity per Square 1.00e+14 ohm
Dielectric Constant 3.2
@Frequency 10000 Hz
Dielectric Strength 160 kV/mmat 0.075 mm
Dissipation Factor 0.0048
@Frequency 10000 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 20.0 - 21.0 µm/m-°C
@Temperature 20.0 °C
biax film
Maximum Service Temperature, Air 155 °C
Flammability, UL94 V-2
Shrinkage 0.80 %
@Temperature 190 °C,
Time 300 sec
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 84 %
@Thickness 0.0750 mm
 
Descriptive Properties
Chemical Resistance - AlcoholsGood
Chemical Resistance - AlkalisGood
Chemical Resistance - AromaticsGood
Chemical Resistance - Concentrated AcidsGood-Poor
Chemical Resistance - Dilute AcidsGood
Chemical Resistance - Greases and OilsGood
Chemical Resistance - HalogensGood
Chemical Resistance - KetonesGood
Permeability to Carbon Dioxide @25°C0.01 x 10-13 cm3.cm cm-2 s-1 Pa -1; (film)
Permeability to Oxygen @25°C0.006 x 10-13 cm3.cm cm-2 s-1 Pa -1; (film)
Permeability to Water @25°C40 x 10-13 cm3.cm cm-2 s-1 Pa -1; (film)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for PEN-PET
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced
Kolon NOPLA® KE131 PEN-PET Copolyester
Mitsui Arlen™ PA MXD6 40% Glass Fiber-Reinforced Modified Nylon 6T (COND)
Mitsui Arlen™ PA MXD6 40% Glass Fiber-Reinforced Modified Nylon 6T (DAM)

PGOODF216 / 42287

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.